Catalog excerpts
Intersmooth 7465Si SPC TBT Free, Low Friction, Self Polishing Copolymer A/F PRODUCT DESCRIPTION A high solids, high performance, TBT free, low friction, self polishing copolymer (SPC) antifouling. Based on patented Silyl Acrylate polymer technology. Particularly suitable for use where solvent emmissions need to be reduced. INTENDED USES Specifically designed for Deep Sea Vessels. For use at Newbuilding or Maintenance & Repair. PRODUCT INFORMATION Colour BEA814-Brown, BEA817-Red Note: The above codes will be substituted by BEA834-Brown and BEA837-Red when supplied from Felling, Dammam and Bangalore manufacturing locations. Finish/Sheen Not applicable Part B (Curing Agent) Not applicable Volume Solids 55% ±2% (ISO 3233:1998) Mix Ratio Not applicable Typical Film Thickness Range: 75 - 150 microns dry (136 - 273 microns wet) may be specified depending upon end use. Theoretical Coverage Range: 7.3 - 3.6 m²/litre at 75 - 150 microns dft, allow appropriate loss factors Method of Application Airless Spray, Brush, Roller Flash Point Single Pack 24°C Induction Period Not applicable Drying Information -5°C 5°C 25°C 35°C Touch Dry [ISO 9117/3:2010] 2 hrs 60 mins 40 mins 30 mins Before Flooding Single Coat 30 hrs 18 hrs 12 hrs 7 hrs Before Flooding Multiple Coats 48 hrs 36 hrs 24 hrs 12 hrs Note For Major Refurbishment and Repair if total dft is >300µm flood times must be increased as follows: 48 hours at 5°C, 36 hours at 25°C and 24 hours at 35°C. Overcoating Data - see limitations Substrate Temperature -5°C Overcoated By Intersmooth 7465Si SPC REGULATORY DATA VOC 5°C 25°C 35°C Min Max Min Max Min Max Min Max 12 hrs 6 mths 6 hrs 6 mths 5 hrs 6 mths 4 hrs 6 mths 394 g/lt as supplied (EPA Method 24) 210 g/kg of liquid paint as supplied. EU Solvent Emissions Directive (Council Directive 1999/13/EC) Note: VOC values are typical and are provided for guidance purposes only. These may be subject to variation depending on factors such as differences in colour and normal manufacturing tolerances. This product does not contain organotin compounds acting as biocides and as such is in compliance with the International Convention on the Control of Harmful Anti-fouling Systems on ships as adopted by IMO in October 2001 (IMO document AFS/CONF/26). Marine Coatings Page 1 of 4 Issue Date:22/12/2011 Ref:4631
Open the catalog to page 1TBT Free, Low Friction, Self Polishing Copolymer A/F SURFACE PREPARATIONS Consult your International Paint representative for details. Consult your International Paint representative for the system best suited for the surfaces to be protected. Use in accordance with the standard Worldwide Marine Specifications. All surfaces to be coated should be clean, dry and free from contamination. High pressure fresh water wash or fresh water wash, as appropriate, and remove all oil or grease, soluble contaminants and other foreign matter in accordance with SSPC-SP1 solvent cleaning. Intersmooth 7465SÌ...
Open the catalog to page 2Intersmooth 7465Si SPC TBT Free, Low Friction, Self Polishing Copolymer A/F APPLICATION Mixing This material is a one pack coating and should always be mixed thoroughly with a power agitator before application. Thinner Not Recommended. Use International GTA007 only in exceptional circumstances (max 5% by volume). DO NOT thin more than allowed by local environmental legislation. Airless Spray Recommended Tip Range 0.54-0.80 mm (21-31 thou) Total output fluid pressure at spray tip not less than 190 kg/cm² (2700 p.s.i.) Conventional Spray Application by conventional spray is not recommended....
Open the catalog to page 3Intersmooth 7465Si SPC TBT Free, Low Friction, Self Polishing Copolymer A/F LIMITATIONS UNIT SIZE Coating lifetime is directly proportional to thickness applied. Performance of the product is dependent upon the specified film thickness being achieved. On immersion, Intersmooth 7465Si SPC will exhibit a slight colour change. Overcoating information is given for guidance only and is subject to regional variation depending upon local climate and environmental conditions. Consult your local International Paint representative for specific recommendations. Apply in good weather. Temperature of...
Open the catalog to page 4All International Marine catalogs and brochures
-
Intergard 5000
4 Pages
-
Formula 150 (MIL-DTL-24441)
4 Pages
-
Interline 975P
4 Pages
-
Interline 994LT
4 Pages
-
Interline 644
4 Pages
-
Interspeed 5617
4 Pages
-
Intersmooth 7670 SPC
4 Pages
-
Interflex 8700 SPC
4 Pages
-
Interplate Zero
4 Pages
-
Intergard 269
4 Pages
-
Interline 850
4 Pages
-
Intersleek 1100SR
4 Pages
-
Intersmooth 7465HS SPC
4 Pages
-
Intersleek 717
4 Pages
-
Interfine 878
4 Pages
-
Intershield 456
4 Pages
-
Intershield 851
4 Pages
-
Intershield 852
4 Pages
-
Intershield 803Plus
4 Pages
-
Intercept 8500LPP PIC
2 Pages
-
Intercept 7000
1 Pages
-
Interbond 808
2 Pages
-
Integard 5555 PIC
2 Pages
-
Silyl acrylate antifoulings
2 Pages
-
Intertrac Vision
4 Pages
-
Intersleek 7180 Linkcoat
6 Pages
-
Intersleek 1000
6 Pages
-
Intershield 5150LWT
2 Pages
-
Intershield 300
8 Pages
-
Interline 9001
6 Pages
-
Interflex 8700 PIC
2 Pages
-
Fisheries
2 Pages
-
Interline 904
2 Pages
-
Intershield 6GV
2 Pages
-
Intershield One-2-One
1 Pages
-
Intersleek 700
2 Pages
-
Interswift 6600
2 Pages
-
Interswift 6800HS
2 Pages
-
Intergard 5400 PIC
2 Pages
-
Interspeed-5640
2 Pages
-
INTERSHIELD 803 DATA SHEET
4 Pages
-
Intershield 300V
4 Pages
-
Intergard 821
4 Pages
-
Intertherm 50
4 Pages
-
INTERTHERM 891 DATA SHEET
4 Pages
-
Intergard 403
4 Pages
-
Universal Primer Range
2 Pages
-
Intersleek
6 Pages
-
Cargo Tank Coatings
7 Pages
-
Antifouling coatings range
8 Pages
-
Cargo Hold Coatings
7 Pages
-
Keeping your fleet protected
6 Pages
-
Intershield_163_Inerta
9 Pages
-
Intercept 8000 LPP
4 Pages
-
Interswift 6900Si
4 Pages
-
Intergard 7500
2 Pages
-
Intergard 7020
2 Pages
-
Intergard 5600 / 5620
2 Pages
-
Interline®9001
5 Pages
-
Interplate® Zero
11 Pages
-
Intersleek7180Brochure
2 Pages
-
Hydroblasting Standards
8 Pages
-
Hydroblasting Standards
15 Pages
-
Maintenance and Repair
19 Pages
-
Slurryblasting Standards
14 Pages
-
Cargo Hold
8 Pages
-
Abrasive Sweep Standards
12 Pages
-
Colour Card
2 Pages
-
Interprime 65
4 Pages
-
Interline 104
4 Pages
-
Intersleek 386
4 Pages
-
Intersleek 737
4 Pages
-
Intersleek 970
4 Pages
-
Intersmooth 360 SPC
4 Pages
-
Intersmooth 7460HS SPC
4 Pages
-
Interspeed 6400
4 Pages
-
Interswift 655
4 Pages
-
Intertuf 362
4 Pages
-
Intershield 163 Inerta 160
4 Pages
-
Intersmooth 365 SPC
4 Pages
-
Interswift 455FB
4 Pages
-
INTERLAC 678
4 Pages
-
INTERGARD 400
4 Pages
-
INTERFINE 629HS
4 Pages
-
INTERZONE 1000 DATA SHEET
4 Pages
-
INTERZINC 22HS DATA SHEET
4 Pages
-
INTERTUF 203 DATA SHEET
4 Pages
-
INTERTHANE 990
4 Pages
-
INTERSHEEN 579 DATA SHEET
4 Pages
-
INTERLAC 665 DATA SHEET
4 Pages
-
INTERGARD 7600 DATA SHEET
4 Pages
-
INTERBOND 501
4 Pages
-
INTERZINC 22 DATA SHEET
4 Pages
-
INTERTUF 262 DATA SHEET
4 Pages
-
INTERSHIELD 300 DATA SHEET
4 Pages
-
INTERPRIME 198
4 Pages
-
INTERGARD 5600 DATA SHEET
4 Pages
-
BALLAST TANK BROCHURE
13 Pages
Archived catalogs
-
Intergard 343
9 Pages