Catalog excerpts
Intersmooth 365 SPC TBT Free Self Polishing Copolymer A/F PRODUCT DESCRIPTION High performance, TBT free, self polishing copolymer (SPC) antifouling system with patented Copper Acrylate technology. INTENDED USES Suitable for use on both Coastal and Deep sea vessels depending on activity profile and intended service life For use at Newbuilding. PRODUCT INFORMATION Colour BEA363-Dark Brown, BEA364-Dark Red, BEA365-Mid Brown, BEA373-Dark Brown, BEA374-Dark Red (Note: BEA373-Dark Brown, BEA374-Dark Red only available in China and specific locations in Europe only - see Worldwide Availability section) Finish/Sheen Not applicable Part B (Curing Agent) Not applicable Volume Solids 40% ±2% (ISO 3233:1998) Typical Film Thickness Range: 70 - 140 microns dry (175 - 350 microns wet) may be specified depending upon end use. Theoretical Coverage Range: 5.7 - 2.9 m²/litre at 70 - 140 microns dft, allow appropriate loss factors Method of Application Airless Spray, Brush, Roller Flash Point Single Pack 22°C (Product produced and supplied in North America has a flashpoint of 21°C due to locally sourced solvents. There is no detrimental effect on product performance.) Drying Information -5°C 25°C 35°C 120 mins 60 mins 40 mins 30 mins 30 hrs 18 hrs 12 hrs 10 hrs -5°C Touch Dry [ISO 9117/3:2010] 5°C 5°C Before Flooding Overcoating Data - see limitations Overcoated By Intersmooth 365 SPC Note REGULATORY DATA Substrate Temperature 25°C 35°C Min Max Min Max Min Max Min Max 12 hrs 6 mths 6 hrs 6 mths 4 hrs 6 mths 3 hrs 6 mths Refer to your International Paint representative for minimum drying time before flooding at higher dry film thickness per coat. VOC 518 g/lt as supplied (EPA Method 24) 343 g/kg of liquid paint as supplied. EU Solvent Emissions Directive (Council Directive 1999/13/EC) Note: VOC values are typical and are provided for guidance purposes only. These may be subject to variation depending on factors such as differences in colour and normal manufacturing tolerances. EPA USA Federal EPA Registration No. 2693-188 (BEA363, BEA364) BEA365 is not approved in the USA This product is not registered in Canada. See Page 4 for additional Regulatory Data. This product does not contain organotin compounds acting as biocides and as such is in compliance with the International Convention on the Control of Harmful Anti-fouling Systems on ships as adopted by IMO in October 2001 (IMO document AFS/CONF/26). Marine Coatings Page 1 of 4 Issue Date:23/08/2011 Ref:78
Open the catalog to page 1Intersmooth 365 SPC TBT Free Self Polishing Copolymer A/F CERTIFICATION When used as part of an approved scheme, this material has the following certification: Product recognised by the following classification societies as compliant with the International Convention on the Control of Harmful Anti-fouling Systems on Ships, 2001 (AFS 2001): • • • • • Lloyds Register Germanischer Lloyd Korean Register of Shipping Det Norske Veritas Bureau Veritas Consult your International Paint representative for details. SYSTEMS AND COMPATIBILITY Consult your International Paint representative for the...
Open the catalog to page 2TBT Free Self Polishing Copolymer A/F Airless Spray This material is a one pack coating. Always mix thoroughly with a power agitator before application. Not Recommended. Use International GTA007 only in exceptional circumstances (max 5% by volume). DO NOT thin more than allowed by local environmental legislation. Total output fluid pressure at spray tip not less than 211 kg/cm2 (3000 p.s.i.) Application by brush is recommended for small areas only. Multiple coats may be required to achieve specified film thickness. Application by roller is recommended for small areas only. Multiple coats...
Open the catalog to page 3Intersmooth 365 SPC TBT Free Self Polishing Copolymer A/F LIMITATIONS Coating lifetime is directly proportional to thickness applied. Performance of the product is dependent upon the specified film thickness being achieved. On immersion, Intersmooth 365 SPC will exhibit a slight colour change. Overcoating information is given for guidance only and is subject to regional variation depending upon local climate and environmental conditions. Consult your local International Paint representative for specific recommendations. Apply in good weather. Temperature of the surface to be coated must be...
Open the catalog to page 4All International Marine catalogs and brochures
-
Intergard 5000
4 Pages
-
Formula 150 (MIL-DTL-24441)
4 Pages
-
Interline 975P
4 Pages
-
Interline 994LT
4 Pages
-
Interline 644
4 Pages
-
Interspeed 5617
4 Pages
-
Intersmooth 7670 SPC
4 Pages
-
Interflex 8700 SPC
4 Pages
-
Interplate Zero
4 Pages
-
Intergard 269
4 Pages
-
Interline 850
4 Pages
-
Intersleek 1100SR
4 Pages
-
Intersmooth 7465HS SPC
4 Pages
-
Intersleek 717
4 Pages
-
Interfine 878
4 Pages
-
Intershield 456
4 Pages
-
Intershield 851
4 Pages
-
Intershield 852
4 Pages
-
Intershield 803Plus
4 Pages
-
Intercept 8500LPP PIC
2 Pages
-
Intercept 7000
1 Pages
-
Interbond 808
2 Pages
-
Integard 5555 PIC
2 Pages
-
Silyl acrylate antifoulings
2 Pages
-
Intertrac Vision
4 Pages
-
Intersleek 7180 Linkcoat
6 Pages
-
Intersleek 1000
6 Pages
-
Intershield 5150LWT
2 Pages
-
Intershield 300
8 Pages
-
Interline 9001
6 Pages
-
Interflex 8700 PIC
2 Pages
-
Fisheries
2 Pages
-
Interline 904
2 Pages
-
Intershield 6GV
2 Pages
-
Intershield One-2-One
1 Pages
-
Intersleek 700
2 Pages
-
Interswift 6600
2 Pages
-
Interswift 6800HS
2 Pages
-
Intergard 5400 PIC
2 Pages
-
Interspeed-5640
2 Pages
-
INTERSHIELD 803 DATA SHEET
4 Pages
-
Intershield 300V
4 Pages
-
Intergard 821
4 Pages
-
Intertherm 50
4 Pages
-
INTERTHERM 891 DATA SHEET
4 Pages
-
Intergard 403
4 Pages
-
Universal Primer Range
2 Pages
-
Intersleek
6 Pages
-
Cargo Tank Coatings
7 Pages
-
Antifouling coatings range
8 Pages
-
Cargo Hold Coatings
7 Pages
-
Keeping your fleet protected
6 Pages
-
Intershield_163_Inerta
9 Pages
-
Intercept 8000 LPP
4 Pages
-
Interswift 6900Si
4 Pages
-
Intergard 7500
2 Pages
-
Intergard 7020
2 Pages
-
Intergard 5600 / 5620
2 Pages
-
Interline®9001
5 Pages
-
Interplate® Zero
11 Pages
-
Intersleek7180Brochure
2 Pages
-
Hydroblasting Standards
8 Pages
-
Hydroblasting Standards
15 Pages
-
Maintenance and Repair
19 Pages
-
Slurryblasting Standards
14 Pages
-
Cargo Hold
8 Pages
-
Abrasive Sweep Standards
12 Pages
-
Colour Card
2 Pages
-
Interprime 65
4 Pages
-
Interline 104
4 Pages
-
Intersleek 386
4 Pages
-
Intersleek 737
4 Pages
-
Intersleek 970
4 Pages
-
Intersmooth 360 SPC
4 Pages
-
Intersmooth 7460HS SPC
4 Pages
-
Intersmooth 7465Si SPC
4 Pages
-
Interspeed 6400
4 Pages
-
Interswift 655
4 Pages
-
Intertuf 362
4 Pages
-
Intershield 163 Inerta 160
4 Pages
-
Interswift 455FB
4 Pages
-
INTERLAC 678
4 Pages
-
INTERGARD 400
4 Pages
-
INTERFINE 629HS
4 Pages
-
INTERZONE 1000 DATA SHEET
4 Pages
-
INTERZINC 22HS DATA SHEET
4 Pages
-
INTERTUF 203 DATA SHEET
4 Pages
-
INTERTHANE 990
4 Pages
-
INTERSHEEN 579 DATA SHEET
4 Pages
-
INTERLAC 665 DATA SHEET
4 Pages
-
INTERGARD 7600 DATA SHEET
4 Pages
-
INTERBOND 501
4 Pages
-
INTERZINC 22 DATA SHEET
4 Pages
-
INTERTUF 262 DATA SHEET
4 Pages
-
INTERSHIELD 300 DATA SHEET
4 Pages
-
INTERPRIME 198
4 Pages
-
INTERGARD 5600 DATA SHEET
4 Pages
-
BALLAST TANK BROCHURE
13 Pages
Archived catalogs
-
Intergard 343
9 Pages