Catalog excerpts
Intersleek 970 Fluoropolymer Foul Release Coating PRODUCT DESCRIPTION A three pack, fluoropolymer foul release coating. INTENDED USES As the finishing coat in the Intersleek 900 foul release system. For use at Newbuilding or Maintenance & Repair. PRODUCT INFORMATION Colour FXA970-White, FXA971-Grey, FXA972-Blue, FXA977-Red, FXA979-Black; and a limited range of colours Finish/Sheen Gloss Part B (Curing Agent) FXA980 (Part B), FXA981 (Part C) Volume Solids 74% ±2% (ISO 3233:1998) Mix Ratio 16 volume(s) Part A to 3 volume(s) Part B to 1 volume(s) Part C Typical Film Thickness Range: 150 - 200 microns dry (203 - 270 microns wet) may be specified depending upon end use. Theoretical Coverage Range: 4.93 - 3.70 m²/litre at 150 - 200 microns dft, allow appropriate loss factors Method of Application Airless Spray, Brush Flash Point Part A 38°C; Part B 24°C; Part C 32°C; Mixed 32°C Induction Period Not required Drying Information 0°C 15°C 25°C 35°C Touch Dry [ISO 9117/3:2010] 7 hrs 4 hrs 3 hrs 2 hrs Hard Dry [ISO 9117-1:2009] 16 hrs 9 hrs 6 hrs 5 hrs Before Flooding 48 hrs 36 hrs 20 hrs 17 hrs 140 mins 90 mins 60 mins 30 mins Pot Life Note The interval prior to flooding may be reduced to 24 hours at temperatures between 5°C and 20°C provided that the ship remains at rest for a minimum period of 2-3 days after flooding. At temperatures between 0°C and 5°C, the absolute minimum time to flooding is 48 hours and the ship must remain at rest for a minimum of 4 days after undocking. However, the coating may suffer intercoat detachment in any areas that are subject to mechanical abrasion due to, eg. fendering or impact damage. Overcoating Data - see limitations Substrate Temperature 0°C Overcoated By Note REGULATORY DATA Min 15°C Max Min 25°C Max Min 35°C Max Min Max May be overcoated by self, either when fresh or after prolonged immersion provided surface is in good, clean condition. Consult International Paint. Intersleek 970 CANNOT be overcoated by Intersleek 757. VOC 248 g/lt as supplied (EPA Method 24) 241 g/kg of liquid paint as supplied. EU Solvent Emissions Directive (Council Directive 1999/13/EC) Note: VOC values are typical and are provided for guidance purposes only. These may be subject to variation depending on factors such as differences in colour and normal manufacturing tolerances. This product does not contain organotin compounds acting as biocides and as such is in compliance with the International Convention on the Control of Harmful Anti-fouling Systems on ships as adopted by IMO in October 2001 (IMO document AFS/CONF/26). Marine Coatings Page 1 of 4 Issue Date:23/09/2011 Ref:3782
Open the catalog to page 1Intersleek 970 Fluoropolymer Foul Release Coating CERTIFICATION When used as part of an approved scheme, this product has the following certification: Product recognised by the following classification societies as compliant with the International Convention on the Control of Harmful Anti-fouling Systems on Ships, 2001 (AFS 2001): • • • • • Lloyds Register Det Norske Veritas Korean Register of Shipping Bureau Veritas Germanischer Lloyd Consult your International Paint representative for details. SYSTEMS AND COMPATIBILITY Consult your International Paint representative for the system best...
Open the catalog to page 2Fluoropolymer Foul Release Coating Airless Spray Conventional Spray Work Stoppages and Cleanup Material is supplied in 3 containers as a unit. Always mix a complete unit in the proportions supplied. (1) Agitate Part A with a power agitator. (2) Combine entire contents of Part A and Part B and mix thoroughly with a power agitator. (3) Add entire contents of Part C and mix thoroughly with a power agitator. Not recommended. Use International GTA007 only in exceptional circumstances. DO NOT thin more than allowed by local environmental legislation. Total output fluid pressure at spray tip not...
Open the catalog to page 3Intersleek 970 Fluoropolymer Foul Release Coating LIMITATIONS Minimum acceptable substrate temperature at the time of application is 0°C. A minimum Relative Humidity of 30% is required to ensure satisfactory curing. Longer cure times will be required if the Relative Humidity falls below 30%. Care should be taken to avoid overspray onto other coated areas. Intersleek 970 must be applied over Intersleek tie coat within the required overcoating interval. All equipment must be thoroughly clean prior to use, and before re-use with other materials, to prevent contamination. Liquid cleaners for...
Open the catalog to page 4All International Marine catalogs and brochures
-
Intergard 5000
4 Pages
-
Formula 150 (MIL-DTL-24441)
4 Pages
-
Interline 975P
4 Pages
-
Interline 994LT
4 Pages
-
Interline 644
4 Pages
-
Interspeed 5617
4 Pages
-
Intersmooth 7670 SPC
4 Pages
-
Interflex 8700 SPC
4 Pages
-
Interplate Zero
4 Pages
-
Intergard 269
4 Pages
-
Interline 850
4 Pages
-
Intersleek 1100SR
4 Pages
-
Intersmooth 7465HS SPC
4 Pages
-
Intersleek 717
4 Pages
-
Interfine 878
4 Pages
-
Intershield 456
4 Pages
-
Intershield 851
4 Pages
-
Intershield 852
4 Pages
-
Intershield 803Plus
4 Pages
-
Intercept 8500LPP PIC
2 Pages
-
Intercept 7000
1 Pages
-
Interbond 808
2 Pages
-
Integard 5555 PIC
2 Pages
-
Silyl acrylate antifoulings
2 Pages
-
Intertrac Vision
4 Pages
-
Intersleek 7180 Linkcoat
6 Pages
-
Intersleek 1000
6 Pages
-
Intershield 5150LWT
2 Pages
-
Intershield 300
8 Pages
-
Interline 9001
6 Pages
-
Interflex 8700 PIC
2 Pages
-
Fisheries
2 Pages
-
Interline 904
2 Pages
-
Intershield 6GV
2 Pages
-
Intershield One-2-One
1 Pages
-
Intersleek 700
2 Pages
-
Interswift 6600
2 Pages
-
Interswift 6800HS
2 Pages
-
Intergard 5400 PIC
2 Pages
-
Interspeed-5640
2 Pages
-
INTERSHIELD 803 DATA SHEET
4 Pages
-
Intershield 300V
4 Pages
-
Intergard 821
4 Pages
-
Intertherm 50
4 Pages
-
INTERTHERM 891 DATA SHEET
4 Pages
-
Intergard 403
4 Pages
-
Universal Primer Range
2 Pages
-
Intersleek
6 Pages
-
Cargo Tank Coatings
7 Pages
-
Antifouling coatings range
8 Pages
-
Cargo Hold Coatings
7 Pages
-
Keeping your fleet protected
6 Pages
-
Intershield_163_Inerta
9 Pages
-
Intercept 8000 LPP
4 Pages
-
Interswift 6900Si
4 Pages
-
Intergard 7500
2 Pages
-
Intergard 7020
2 Pages
-
Intergard 5600 / 5620
2 Pages
-
Interline®9001
5 Pages
-
Interplate® Zero
11 Pages
-
Intersleek7180Brochure
2 Pages
-
Hydroblasting Standards
8 Pages
-
Hydroblasting Standards
15 Pages
-
Maintenance and Repair
19 Pages
-
Slurryblasting Standards
14 Pages
-
Cargo Hold
8 Pages
-
Abrasive Sweep Standards
12 Pages
-
Colour Card
2 Pages
-
Interprime 65
4 Pages
-
Interline 104
4 Pages
-
Intersleek 386
4 Pages
-
Intersleek 737
4 Pages
-
Intersmooth 360 SPC
4 Pages
-
Intersmooth 7460HS SPC
4 Pages
-
Intersmooth 7465Si SPC
4 Pages
-
Interspeed 6400
4 Pages
-
Interswift 655
4 Pages
-
Intertuf 362
4 Pages
-
Intershield 163 Inerta 160
4 Pages
-
Intersmooth 365 SPC
4 Pages
-
Interswift 455FB
4 Pages
-
INTERLAC 678
4 Pages
-
INTERGARD 400
4 Pages
-
INTERFINE 629HS
4 Pages
-
INTERZONE 1000 DATA SHEET
4 Pages
-
INTERZINC 22HS DATA SHEET
4 Pages
-
INTERTUF 203 DATA SHEET
4 Pages
-
INTERTHANE 990
4 Pages
-
INTERSHEEN 579 DATA SHEET
4 Pages
-
INTERLAC 665 DATA SHEET
4 Pages
-
INTERGARD 7600 DATA SHEET
4 Pages
-
INTERBOND 501
4 Pages
-
INTERZINC 22 DATA SHEET
4 Pages
-
INTERTUF 262 DATA SHEET
4 Pages
-
INTERSHIELD 300 DATA SHEET
4 Pages
-
INTERPRIME 198
4 Pages
-
INTERGARD 5600 DATA SHEET
4 Pages
-
BALLAST TANK BROCHURE
13 Pages
Archived catalogs
-
Intergard 343
9 Pages