Intersmooth 7460HS SPC - 1

Intersmooth 7460HS SPC TBT Free, Low Friction, Self Polishing Copolymer A/F PRODUCT DESCRIPTION A high solids, high performance, TBT free, low friction, self polishing copolymer (SPC) antifouling. Particularly suitable for use where solvent emissions need to be reduced. INTENDED USES Specifically designed for Deep Sea Vessels. For use at Maintenance & Repair. PRODUCT INFORMATION Colour BEA754-Brown, BEA757-Red, BEA751-Black BEA744-Brown, BEA747-Red (only available in European non-regulated countries) Finish/Sheen Not applicable Part B (Curing Agent) Not applicable Volume Solids 54% ±2% (ISO 3233:1998) Mix Ratio Not applicable Typical Film Thickness Range: 75 - 200 microns dry (139 - 370 microns wet) may be specified depending upon end use. Theoretical Coverage Range: 7.2 - 2.7 m²/litre at 75 - 200 microns dft, allow appropriate loss factors Method of Application Airless Spray, Brush, Roller Flash Point Single Pack 25°C Drying Information -5°C 25°C 35°C 120 mins 60 mins 40 mins 30 mins 30 hrs 20 hrs 16 hrs 10 hrs 48 hrs Touch Dry [ISO 9117/3:2010] 5°C 36 hrs 24 hrs Before Flooding 0-36 Month Schemes Before Flooding 48-60 Month Schemes Note For 0-36 month schemes the times before flooding must revert to the times for 48-60 month schemes if: 1) the antifouling scheme includes any single coat greater than 150 microns, and 2) the vessel service speed is greater than 15 knots For 48-60 month schemes the times before flooding can revert to the times for 0-36 month schemes if: 1) no single coat is applied at more than 150 microns, or 2) the vessel service speed is less than 15 knots Overcoating Data - see limitations Substrate Temperature -5°C Overcoated By Intersmooth 7460HS SPC 0-36 Month Schemes Intersmooth 7460HS SPC 48-60 Month Schemes REGULATORY DATA VOC 5°C 25°C 35°C Min Max Min Max Min Max Min Max 12 hrs 28 days 6 hrs 28 days 4 hrs 28 days 3 hrs 28 days - - 18 hrs 28 days 12 hrs 28 days 9 hrs 28 days 425 g/lt as supplied (EPA Method 24) 226 g/kg of liquid paint as supplied. EU Solvent Emissions Directive (Council Directive 1999/13/EC) Note: VOC values are typical and are provided for guidance purposes only. These may be subject to variation depending on factors such as differences in colour and normal manufacturing tolerances. EPA This product is not registered in the USA or Canada. This product does not contain organotin compounds acting as biocides and as such is in compliance with the International Convention on the Control of Harmful Anti-fouling Systems on ships as adopted by IMO in October 2001 (IMO document AFS/CONF/26). Marine Coatings Page 1 of 4 Issue Date:25/11/2011 Ref:3719

カタログの1ページ目を開く
Intersmooth 7460HS SPC - 2

Intersmooth 7460HS SPC TBT Free, Low Friction, Self Polishing Copolymer A/F CERTIFICATION Consult your International Paint representative for details. SYSTEMS AND COMPATIBILITY Consult your International Paint representative for the system best suited for the surfaces to be protected. SURFACE PREPARATIONS Use in accordance with the standard Worldwide Marine Specifications. All surfaces to be coated should be clean, dry and free from contamination. High pressure fresh water wash or fresh water wash, as appropriate, and remove all oil or grease, soluble contaminants and other foreign matter...

カタログの2ページ目を開く
Intersmooth 7460HS SPC - 3

Intersmooth 7460HS SPC TBT Free, Low Friction, Self Polishing Copolymer A/F APPLICATION Mixing This material is a one pack coating and should always be mixed thoroughly with a power agitator before application. Thinner Not Recommended. Use International GTA007 only in exceptional circumstances (max 5% by volume). DO NOT thin more than allowed by local environmental legislation. Airless Spray Recommended Tip Range 0.54-0.80 mm (21-31 thou) Total output fluid pressure at spray tip not less than 190 kg/cm² (2700 p.s.i.) Conventional Spray Application by conventional spray is not recommended....

カタログの3ページ目を開く
Intersmooth 7460HS SPC - 4

Intersmooth 7460HS SPC TBT Free, Low Friction, Self Polishing Copolymer A/F LIMITATIONS UNIT SIZE Coating lifetime is directly proportional to thickness applied. Performance of the product is dependent upon the specified film thickness being achieved. On immersion, Intersmooth 7460HS SPC will exhibit a slight colour change. Overcoating information is given for guidance only and is subject to regional variation depending upon local climate and environmental conditions. Consult your local International Paint representative for specific recommendations. Apply in good weather. Temperature of...

カタログの4ページ目を開く

International Marineのすべてのカタログとパンフレット

  1. Intergard 5000

    4 ページ

  2. Interline 975P

    4 ページ

  3. Interline 994LT

    4 ページ

  4. Interline 644

    4 ページ

  5. Interspeed 5617

    4 ページ

  6. Interflex 8700 SPC

    4 ページ

  7. Interplate Zero

    4 ページ

  8. Intergard 269

    4 ページ

  9. Interline 850

    4 ページ

  10. Intersleek 1100SR

    4 ページ

  11. Intersleek 717

    4 ページ

  12. Interfine 878

    4 ページ

  13. Intershield 456

    4 ページ

  14. Intershield 851

    4 ページ

  15. Intershield 852

    4 ページ

  16. Intercept 7000

    1 ページ

  17. Interbond 808

    2 ページ

  18. Integard 5555 PIC

    2 ページ

  19. Intertrac Vision

    4 ページ

  20. Intersleek 1000

    6 ページ

  21. Intershield 300

    8 ページ

  22. Interline 9001

    6 ページ

  23. Interflex 8700 PIC

    2 ページ

  24. Fisheries

    2 ページ

  25. Interline 904

    2 ページ

  26. Intershield 6GV

    2 ページ

  27. Intersleek 700

    2 ページ

  28. Interswift 6600

    2 ページ

  29. Interswift 6800HS

    2 ページ

  30. Intergard 5400 PIC

    2 ページ

  31. Interspeed-5640

    2 ページ

  32. Intershield 300V

    4 ページ

  33. Intergard 821

    4 ページ

  34. Intertherm 50

    4 ページ

  35. Intergard 403

    4 ページ

  36. Intersleek

    6 ページ

  37. Intercept 8000 LPP

    4 ページ

  38. Interswift 6900Si

    4 ページ

  39. Intergard 7500

    2 ページ

  40. Intergard 7020

    2 ページ

  41. Interline®9001

    5 ページ

  42. Interplate® Zero

    11 ページ

  43. Cargo Hold

    8 ページ

  44. Colour Card

    2 ページ

  45. Interprime 65

    4 ページ

  46. Interline 104

    4 ページ

  47. Intersleek 386

    4 ページ

  48. Intersleek 737

    4 ページ

  49. Intersleek 970

    4 ページ

  50. Interspeed 6400

    4 ページ

  51. Interswift 655

    4 ページ

  52. Intertuf 362

    4 ページ

  53. Interswift 455FB

    4 ページ

  54. INTERLAC 678

    4 ページ

  55. INTERGARD 400

    4 ページ

  56. INTERFINE 629HS

    4 ページ

  57. INTERTHANE 990

    4 ページ

  58. INTERBOND 501

    4 ページ

  59. INTERPRIME 198

    4 ページ

カタログアーカイブ

  1. Intergard 343

    9 ページ