Product Data HEMPEL'S ALUSAFE 7120D Description: HEMPEL'S ALUSAFE 7120D is a copper-free self polishing sntifouling with organic bioactive material. It changes to final colour after approximately 1 week of exposure to water. Due to its self-renewing effect this product maintains an effective bioactive surface during its entire sefvice life. Recommended use: As an antifouling for boats of aluminium and other light-alloy metal. Primarily for use in water with relatively low fouling potential. Length of service may have a certain influence on colour. The antifouling may obtain a greenish tinge. For cold and temperate waters. Availability: Subject to special agreement. PHYSICAL CONSTANTS: Shade nos/Colours: Finish: Volume solids, %: Theoretical spreading rate: Flash point: Specific gravity: Dry to touch: VOC content: - 10000*/ White. Semi-flat 54 ± 1 13.5 m2/l [541.4 sq.ft./US gallon] - 40 micron/1.6 mils 32 °C [89.6 °F] 1.5 kg/litre [12.6 lbs/US gallon] 4 approx. hour(s) 20°C/68°F 8 (approx.) hrs at 10°C/50°F 399 g/l [3.3 lbs/US gallon] *other shades according to assortment list. The physical constants stated are nominal data according to the HEMPEL Group's approved formulas. APPLICATION DETAILS: Application method: Thinner (max.vol.): Nozzle orifice: Nozzle pressure: Cleaning of tools: Indicated film thickness, dry: Indicated film thickness, wet: Recoat interval, min: Recoat interval, max: Safety: Date of issue: January 2012 - Airless spray / Air spray / Brush/Roller/Paint pad 08080 (5%) / 08080) (15%) / 08080 (5%) 0.018 - 0.023 " 150 bar [2175 psi] (Airless spray data are indicative and subject to adjustment) HEMPEL'S THINNER 08080 40 micron [1.6 mils] see REMARKS overleaf. 75 micron [3 mils] According to specification. According to specification. Handle with care. Before and during use, observe all safety labels on packaging and paint containers, consult HEMPEL Safety Data Sheets and follow all local or national safety regulations. Page: 1/2 Product Data Sheet
カタログの1ページ目を開く
HEMPEL'S ALUSAFE 7120D SURFACE PREPARATION: Existing old self-polishing or ablative antifouling: Remove possible oil and grease etc. with suitable detergent, followed by high pressure fresh water cleaning for a thorough removal of any possible weak structure of leached antifouling. Allow the surface to dry before coating. Sealer: Whether to use a sealer coat/tiecoat or not depends on the type and condition of the existing antifouling. APPLICATION CONDITIONS: The surface must be completely clean and dry at the time of application and its temperature must be above the dew point to avoid...
カタログの2ページ目を開くHempelのすべてのカタログとパンフレット
-
Hempadur 85671
2 ページ
-
Hempasil X3+
2 ページ
-
Globic 9000 78950
2 ページ
-
Olympic+ 72950
2 ページ
-
Dynamic 9000 79900
2 ページ
-
HEMPAGUARD X5 89700
2 ページ
-
HEMPAGUARD X7 89900
2 ページ
-
PDS HEMPADUR 17630
2 ページ
-
PDS HEMPADUR 15570
2 ページ
-
PDS HEMPADUR 15500
2 ページ
-
PDS HEMPADUR 15400
2 ページ
-
PDS GLOBIC 9000
2 ページ
-
PDS GLOBIC 6000
2 ページ
-
HEMPADUR 15553
2 ページ
-
HEMPADUR 15590
2 ページ
-
HEMPADUR 35560
2 ページ
-
HEMPASIL NEXUS 27302
2 ページ
-
HEMPASIL X3 87500
2 ページ
-
HEMPASIL BROCHURE
12 ページ